Sales Manager, U.S. and Canada
- FMA
- The Fabricator
- FABTECH
- Canadian Metalworking
Categories
- Additive Manufacturing
- Aluminum Welding
- Arc Welding
- Assembly and Joining
- Automation and Robotics
- Bending and Forming
- Consumables
- Cutting and Weld Prep
- Electric Vehicles
- En Español
- Finishing
- Hydroforming
- Laser Cutting
- Laser Welding
- Machining
- Manufacturing Software
- Materials Handling
- Metals/Materials
- Oxyfuel Cutting
- Plasma Cutting
- Power Tools
- Punching and Other Holemaking
- Roll Forming
- Safety
- Sawing
- Shearing
- Shop Management
- Testing and Measuring
- Tube and Pipe Fabrication
- Tube and Pipe Production
- Waterjet Cutting
Industry Directory
Webcasts
Podcasts
FAB 40
Advertise
Subscribe
Account Login
Search
What electromechanical gap control means for metal leveling
Metal fabricators don’t have to worry about maintenance related to hydraulics
- By Dennis Ebner
- September 21, 2023
- Article
- Laser Cutting
Achieving flat and stress-free sheets or parts is essential in the metalworking industry for ensuring high-quality manufacturing.
Roll leveling is a key process that eliminates flatness defects and internal stresses. Traditionally, hydraulic systems have been employed to control the leveling gap and counter the forces exerted during the leveling process. Today, leveling technology centered on electromechanical gap control is available and has the potential to minimize maintenance concerns and energy consumption.
The Principle of Leveling With Rollers
Roll leveling is commonly used for both metal strips and flat metal parts, allowing for the removal of unevenness and tensions introduced during coil winding or previous treatments. Roll leveling machines employ upper and lower leveling rollers arranged in an offset configuration to guide the material through a serpentine-like line. This process involves initially bending the material beyond its yield strength, heavily plasticizing it and thereby eliminating undesired bends and tensions. Subsequently, as the material continues through the machine, it is bent a little less on each further leveling roller until the material is no longer plasticized by the time it reaches the last leveling roller, only deformed elastically. During this process, adjustable leveling gaps play a crucial role in accommodating variations in material thickness or bending moments, ensuring optimal leveling results.
Challenges in Leveling Gap Control
As the material passes through the leveling gap, high counterforces arise within the machine. These forces tend to expand or open the leveling gap, necessitating robust design considerations for the rods and bolts that hold the machine frame in the desired position relative to one another. Previous approaches from manufacturers involved oversized components to withstand the forces, leading to increased weight and manufacturing costs.
Hydraulic systems have been conventionally used to compensate for the elongation of rods and maintain the leveling gap in part leveling machines. While hydraulic piston-cylinder units offer the required forces and response time, these systems can be considered complex and require regular maintenance. Some users also have concerns over their energy consumption.
To address the challenges associated with hydraulic adjustment devices in metal leveling, an electromechanical gap control system has been developed. This system replaces hydraulic components with electromechanically operated sliding wedges, providing advantages in machine structure, manufacturing costs, and maintenance requirements.
The electromechanical gap control system employs an electric motor, such as a three-phase servo drive, to drive the movement of the sliding wedge. Typically, this electric motor is coupled with a gear system, like a worm gear, which interfaces with a spindle responsible for displacing the sliding wedge. By using an electric servomotor, direct interaction with sensors or monitoring devices becomes possible. This enables real-time compensation of changes in the effective length of the rods. The adjustment mechanism simplifies control through conventional electrical systems, leveraging control electronics and sensor feedback for precise control over the amount of force applied, allowing for accurate and consistent leveling.
Benefits of Electromechanical Gap Control
The electromechanical gap control system eliminates the need for hydraulic components, reducing energy consumption and maintenance costs. The sliding wedge design also generates high vertical forces with minimal horizontal forces, ensuring precise and efficient adjustment. Additionally, the system provides overload protection by limiting the compensation of rod elongation, safeguarding the leveling machine and its components, such as cardan shafts, from potential damage.
Overload Protection
Electromechanical gap control provides a protective mechanism for the leveling machine when it is at risk of overstress or overload. Even in situations where the forces in the leveling gap reach potentially damaging levels, the electromechanical system can prevent material plasticization by partially reducing the compensation of rod elongation based on material-specific calculations. The independent movement of sliding wedges for each rod allows for this adjustment. While the leveling result for the current sheet or part might not be optimal, it is often still usable, effectively safeguarding the leveling machine against overload.
Mechanical Adjustments and Hydraulic Pressure
Although some believe that thin metals require a mechanical adjustment while thick metals necessitate hydraulic pressure, they are not correct. The choice between mechanical adjustment and hydraulic pressure is not solely dependent on the thickness of the metal being leveled.
In the leveling process, the pressure requirements (tonnage) needed to destress and level material are influenced by various factors such as the material's properties, surface conditions, and the desired leveling outcome. While it is true that thin metals generally exert lower tonnage requirements compared to thicker metals, the choice between mechanical adjustment and hydraulic pressure should not be solely based on metal thickness.
Modern electromechanical gap control systems provide an effective and versatile solution for both thin and thick metals. Nonhydraulic machines are currently available that can handle metal thicknesses ranging from 0.024 in. (0.6 mm) to 2.6 in. (66 mm). These systems utilize servomotors and sliding wedges to precisely control the leveling gap, regardless of the material thickness. By monitoring the forces and adjusting the effective length of the rods, electromechanical systems can accommodate the specific requirements of the leveling process across a wide range of metal thicknesses.
Electromechanical systems can achieve high levels of power density and efficiency, providing fast response times and precise positioning capabilities.
About the Author
Related Companies
subscribe now
The Fabricator is North America's leading magazine for the metal forming and fabricating industry. The magazine delivers the news, technical articles, and case histories that enable fabricators to do their jobs more efficiently. The Fabricator has served the industry since 1970.
start your free subscription- Stay connected from anywhere
Easily access valuable industry resources now with full access to the digital edition of The Fabricator.
Easily access valuable industry resources now with full access to the digital edition of The Welder.
Easily access valuable industry resources now with full access to the digital edition of The Tube and Pipe Journal.
Easily access valuable industry resources now with full access to the digital edition of The Fabricator en Español.
- Podcasting
- Podcast:
- The Fabricator Podcast
- Published:
- 05/14/2024
- Running Time:
- 62:12
Cameron Adams of Laser Precision, a contract metal fabricator in the Chicago area, joins the podcast to talk...
- Trending Articles
Why employee-owned companies make sense in manufacturing
What software automation means for custom fabrication
Nucor’s weekly steel price announcement continues to rattle markets
Press brakes, panel benders, and flat blank calculations
Washington artist creates life-size elk sculptures
- Industry Events
Laser Welding Certificate Course
- May 7 - August 6, 2024
- Farmington Hills, IL
World-Class Roll Forming Workshop
- June 5 - 6, 2024
- Louisville, KY
Advanced Laser Application Workshop
- June 25 - 27, 2024
- Novi, MI
Precision Press Brake Certificate Course
- July 31 - August 1, 2024
- Elgin,